[1]石祥,黄丽红,龚凌诸,等.常减压装置含缺陷管道安全评定分析[J].福建工程学院学报,2023,21(01):6-13.[doi:10.3969/j.issn.1672-4348.2023.01.002]
 SHI Xiang,HUANG Lihong,GONG Lingzhu,et al.Safety assessment analysis of pipes with defects in atmospheric anddecompression devices[J].Journal of FuJian University of Technology,2023,21(01):6-13.[doi:10.3969/j.issn.1672-4348.2023.01.002]
点击复制

常减压装置含缺陷管道安全评定分析()
分享到:

《福建工程学院学报》[ISSN:2097-3853/CN:35-1351/Z]

卷:
第21卷
期数:
2023年01期
页码:
6-13
栏目:
出版日期:
2023-02-25

文章信息/Info

Title:
Safety assessment analysis of pipes with defects in atmospheric anddecompression devices
作者:
石祥黄丽红龚凌诸苏宣机黄耀波朱猛
福建工程学院生态环境与城市建设学院
Author(s):
SHI Xiang HUANG Lihong GONG Lingzhu SU Xuanji HUANG Yaobo ZHU Meng
School of Ecological Environment and Urban Construction, Fujian University of Technology
关键词:
缺陷常减压装置管道安全评定
Keywords:
defect atmospheric and decompression pressure device pipeline safety assessment
分类号:
TQ055.8
DOI:
10.3969/j.issn.1672-4348.2023.01.002
文献标志码:
A
摘要:
以某常减压装置含缺陷管道为研究对象,采用超声相控阵检测方法对管道焊接接头进行无损检测,确定管道缺陷类型和尺寸,根据GB/ T 19624—2019 推荐的安全评定方法对管道缺陷进行安全评定,通过改变缺陷的大小和间距,探究缺陷类型、尺寸和相互位置对管道安全评定的影响,结果表明:裂纹缺陷单独存在时,缺陷高度对安全评定影响最大;未焊透缺陷单独存在时,缺陷长度对安全评定影响最大;两条缺陷共存时,随着缺陷间距S的增大,缺陷处应力先缓慢增大后快速减小并逐步趋于稳定,但是由于管道中缺陷数量增加,导致两条单独存在时均安全的缺陷在共存时可能造成管道不安全。
Abstract:
The defective pipes in an atmospheric and decompression device were selected as the research object. The ultrasonic phased array detection method was adopted to conduct nondestructive testing on welded joints of pipelines to determine the type and size of pipeline defects. The pipeline defects were assessed according to the safety assessment method recommended by GB/T 196242019. By changing the size and spacing of defects, the influence of defect type, size and mutual location on pipeline safety assessment was investigated. Results show that the height of flaw has the greatest influence on pipeline safety evaluation when the crack defect exists alone. The length of defect has the greatest influence on the safety evaluation when there is incomplete penetration defect alone. When the two defects coexist, with the increase of defect spacing S, the stress at the defect increases slowly first, then decreases rapidly and gradually becomes stable. However, due to the increase in the number of defects in the pipeline, the two defects that are both safe when they exist alone may cause pipeline insecurity when they coexist.

参考文献/References:

[1]张华. 压力管道焊接接头裂纹原因分析[J]. 中国设备工程,2022(13):164-166. [2]方学锋,张伯君,梁斌,等. 高温蒸汽管道焊接接头缺陷分析与安全评定[J]. 炼油与化工,2020,31(4):53-55. [3]王海锋,郭涛,周海彦. 在用含未焊透缺陷工业管道的安全评定[J]. 管道技术与设备,2021(1):6-8. [4]李建锋,周昌宗. 含未熔合缺陷压力管道安全评定[J]. 石化技术,2022,29(8):27-29. [5]国家市场监督管理总局,国家标准化管理委员会. 在用含缺陷压力容器安全评定:GB/T 19624—2019[S]. 北京:中国标准出版社,2019. [6]张皓,郑朋刚. 压力管道的分析、评定和检测[J]. 化工管理,2018(27):216-217. [7]北京兆迪科技有限公司. ANSYS Workbench 19.0结构分析从入门到精通[M]. 北京:机械工业出版社,2019:326. [8]程新宇,冯晓伟,李治贵,等. 基于ANSYS/WORKBENCH的压力容器接管应力分析[J]. 石油和化工设备,2011,14(2):5-8. [9]铁摩辛柯,古地尔.弹性理论[M]. 徐芝纶,译. 北京:高等教育出版社,2013:523. [10]黄昆. 在用含缺陷压力管道的安全性分析[J]. 机电技术,2013,36(4):149-153.